KH-540 3-Aminopropyltrimethoxysilane

price : $
  • 品牌 : Epoxy
  • time : 2021.06.08

Nub:




  • product introduction
  • message

 

KH-540 3-Aminopropyltrimethoxysilan

Description:


Chemical Name:3-Aminopropyltrimethoxysilane
Molecular Formula:H2N(CH2)3Si(OCH3)3


Structural Formula:540.png
Molecular Weight:179.29
CAS No.:13822-56-5


Physical Properties


Physical Form:Transparent liquid

Color:Colorless or slightly yellow

Specific Gravity at 25/25℃:1.0160±0.0050

Boiling Point,℃:91-92/15mmHg

Refractive Index, nD 25℃:1.4240±0.005

Flash Point, Pensky-Martens Closed Cup(1),℃:


Applications


"When used in thermoplastic and thermosetting resin such as phenol aldehyde, polyester, epoxy, PBT, polyamide, carbonate, KH-540 can greatly improve dry and wet bending strength, compression strength, shear strength and other physical mechanical properties, and wet electric properties. KH-540 also improves the wetting property and dispersion of stuffing into polymer.
When used in the sand casting of resin, KH-540 can strengthen the adhesion, improve profile sand strength and antiwetting property. When added into phenol aldehyde in the production of glass fibre cotton and mineral cotton, it can improve moisture proof property and strengthen compression elastic resilience.
KH-540 is an excellent adhesion improver used in polyamide, epoxy, nitrile, phenol aldehyde adhesive and sealed material. KH-540 improves the dispersion of pigment and the adhesion to glass, aluminum, iron, also applicable for latex coating such as polyamide, epoxy and acrylic acid type."     

                               

Packaging and Storage


Be packed in 25KG, 200KG drums, IBC and ISO Tank.                                    
Be sealed and stored in cool and well ventilated place. Away from fire and water.

 

 

Application Fields