KH-560 3-Glycidoxypropyltrimethoxysilane


Description:


Chemical Name:3-Glycidoxypropyltrimethoxysilane
Molecular Formula:C9H20O5Si
Structural Formula:560.png
Molecular Weight:236.3 
CAS No.:2530-83-8


Physical Properties


Physical Form:Transparent liquid

Color:Colorless

Specific Gravity at 25/25℃:1.07

Boiling Point,℃:262

Refractive Index, nD 25℃:1.426-1.428

Flash Point, Pensky-Martens Closed Cup(1),℃:122


Applications


KH-560 is a kind of coupling agent with epoxy group. It can be used as caulking glue or sealant of polysulfide and polyurethane, adhesive of epoxy resin, and also can be used in thermosetting resin of filling or reinforcement mode, glass fiber adhesive and thermoplastic resin of inorganic filler or glass reinforcement, etc.
Improve intensity properties of hard composite materials which use glass fiber roving as reinforcement. Keep intensity at maximum point after humidity period. Enhance electrical properties of epoxy resin-based sealants, packaging materials, and printed circuit boards. It is the result of improving the adhesiveness between fillers or between resin and matrix. Enhance electrical properties of composite materials of inorganic filling, including nylon and polybutylene terephthalate.
Be effiective to various fillers, matrix, clay, talc, aedelforsite, silica and quartz, or metals like aluminum, cooper and iron.
Improve cohesiveness of caulking glue and sealant, with water containing acrylic latex, used in polyurethane and epoxy resin coatings. It can improve the solubility, dispersity and fluidity of adhesive when put it into the organic toner.


Packaging and Storage


Be packed in 25KG, 200KG drums, IBC and ISO Tank.                                    
Be sealed and stored in cool and well ventilated place. Away from fire and water.

 