KH-605 yltriamine propylmethyldimethoxyl silane
Description: Chemical Name:γ-divinyltriamine propylmethyldimethoxyl silane Molecular Formula:C10H27N3O2Si Structural Formula: Molecular Weight:249.4 CAS No.:99740-64-4
Physical Properties
Physical Form:Oily liquid Color:Light yellow Specific Gravity at 25/25℃:0.97±0.01 Boiling Point,℃:293-302 Refractive Index, nD 25℃:1.4585-1.4615 Flash Point, Pensky-Martens Closed Cup(1),℃:144.5
Applications "Hydrocarbyl amine alkoxy is a kind of widely used silane coupling agent, especially used as raw materials of silicone microemulsion and emulsions in the textile industry. CG-605 is a the amino silane coupling agent which is modified by diethylenetriamine. It's mico-emulsions and emulsion are used as softening agent of cotton, linen, wool, silk and chemical fiber fabric, and it makes the fabric to be soft, smooth, fluffy and elastic. "
Packaging and Storage Be packed in 25KG, 200KG drums, IBC and ISO Tank. Be sealed and stored in cool and well ventilated place. Away from fire and water.
|